                                                      SPC INSTALLATION GUIDELINES




                               Indoor temperature : SPC  oor is suitable for indoor environment, not suitable for outdoor environment where
                               exposed to sunlight and driving. After the  oor arrives at the site, it should be left unpacked for 24-48 hours to acclimate

                               to let the thermal expansion and contraction rate of the  oor same as the new environment.
                               The room temperature should be controlled between 18-29 degrees Celsius to avoid sun exposure before installation.




                               Flatness : The paving of SPC  oor requires a higher level of  atness of the sub  oor. Often the  atness of the sub  oor
                               directly determines whether the SPC  oor can be used.
                               Therefore, when deciding to use the SPC  oor, the original ground must be leveling (terrazzo, ceramic tiles,  oor paint,
                               etc. can be laid directly), Sub  oor should be  at within a tolerance of 3mm per 2 meter , otherwise, self-leveling cement
                                         Underlayment: It is recommended to use
                               should be used for leveling.

                                         1.0mm underlayment, and it is forbidden to
                               Underlayment :  It is recommended to use 1.0mm underlayment, and it is forbidden  to  use
                                         use underlayment over 2.0mm. Especially for
                               underlayment over 2.0mm. Especially for SPC  oors with a thickness of 4MM,if  the sub  oor
                               uneven, underlayment too thick, which can easily cause the click to break and trip.
                                         SPC  oors with a thickness of 4MM,if the sub

                                          oor uneven, underlayment too thick, which
                               Allow a minimum 8-10MM gap between SPC  oor and wall for spc  oor expansion. If the room is
                               particularly long and wide, the gap should be widened accordingly or T-molding should be used
                                         can easily cause the click to break and trip.
                               as partitions if the length or width greater than 10 meter.
                               Insu cient reserved gap can easily cause  oor arching and tile like deformation.




                               Accessories : Reducer, Quarter round, T-moulding should not prevent the  oor from  oating.
                               Even  no  heavy  furniture  should  be  placed  on  the   ooring  as  this  will  block  the   oor  from

                               expansion and contraction.



                               Maintenance : SPC  oor does not need special maintenance, regular cleaning is enough.
                               Avoid exposure to direct sunlight for prolonged periods of time. Do not roll or drag heavy objects
                               across your  oor. Do not polish or wax or steam clean the  oor.
   2   3   4   5   6   7   8   9